  1. Recommended annealing temperature for TP321 and 321 wrought stainless steel: 1040 °C (1900 °F); Minimum 1095 °C (2000 °F) for cold-worked 321H and 1050 °C (1095 °F) for hot-finished 321H. Stress-relieving treatments. For dimensional stability: Stress relieve at 205 to 480 °C (400 to 900 °F) and then slow cool (usual time, 4 h per inch ...

  2. Stainless steel, also known as inox, corrosion-resistant steel ( CRES) and rustless steel, is an alloy of iron that is resistant to rusting and corrosion. It contains iron with chromium and other elements such as molybdenum, carbon, nickel and nitrogen depending on its specific use and cost. Stainless steel's resistance to corrosion results ...

  3. People also ask

  4. Jan 10, 2023 · 321 Stainless Steel Composition. UNS S32100 composition is an ideal choice for Inconel sheet applications. It has excellent high-temperature strength, good corrosion resistance, and forming ability, as well as great weldability. Other benefits of its composition include high resistance to scaling from heating in high-temperature environments ...

  5. Oct 23, 2001 · Grades 321 and 347 are the basic austenitic 18/8 steel (Grade 304) stabilized by Titanium (321) or Niobium (347) additions. These grades are used because they are not sensitive to intergranular corrosion after heating within the carbide precipitation range of 425-850 °C. Grade 321 is the grade of choice for applications in the temperature ...

  6. Corrosion Resistance. 321 stainless steel exhibits good general corrosion resistance, and excellent resistance to intergranular corrosion after exposure to temperatures in the chromium carbide precipitation range of 800 – 1500°F (427 – 816°C), 321 resists oxidation to 1500°F (816°C) and has higher creep and stress rupture properties than alloys 304 and 304L.

  7. Aug 15, 2023 · 321 stainless steel is a Ni-Cr-Ti austenitic stainless steel used in the manufacture of acid-resistant containers and wear-resistant equipment linings and pipelines. Japanese grade: SUS321. UK grade: 304S12, 321920. German grade: X10CrNiTi189. Also known as: Austenitic Stainless Steel.

  8. Type 321 is a stabilized austenitic stainless steel similar to type 304 but with a titanium addition. This titanium addition reduces or prevents carbide precipitation during welding and in 800 - 1500 °F (427 - 816 °C) service. It also improves the elevated temperature properties of the alloy. Type 321 provides excellent resistance to ...